PROBLEM TO BE SOLVED: To improve flame retardancy, tracking resistance, insulation resistance and water absorption by impregnating a paper base material into a resin varnish for a first coat containing a water-soluble phenol resin and a nitrogen-containing water-soluble resin followed by impregnating a thermosetting resin varnish. ;SOLUTION: A paper base material is impregnated into a resin varnish for a first coat having 8-15 wt.% of nitrogen content in a solid water-soluble resin composed of a water-soluble phenol resin and a nitrogen-containing water-soluble resin in a molecule so that an adhesive amount of the first coat resin becomes 10-25 wt.% after drying, followed by drying. Next, the paper base material is impregnated into a resin varnish for a final coat composed of a thermosetting resin varnish such as a phenol resin, an epoxy resin, a melamine resin and an unsaturated polyester resin so that the total adhesive amount with the resin varnish for the first coat becomes 45-60 wt.%, preferably 50-55 wt.% after drying, followed by drying.;COPYRIGHT: (C)2000,JPO
机译:要解决的问题:为了提高阻燃性,耐漏电性,绝缘电阻和吸水率,将纸基材料浸渍到用于包含水溶性酚醛树脂和含氮水溶性树脂的第一涂层的树脂清漆中,然后浸渍热固性树脂清漆。 ;解决方案:将纸基材料浸渍到用于第一涂料的树脂清漆中,该涂料的固溶性水溶性树脂中的氮含量为8-15 wt。%,该水溶性树脂由水溶性酚醛树脂和含氮水溶性树脂组成干燥后,第一涂层树脂的粘合量变为10-25重量%。接着,将纸基材浸入用于由酚醛树脂,环氧树脂,三聚氰胺树脂和不饱和聚酯树脂等热固性树脂清漆组成的最终涂层用树脂清漆中,以使其与树脂清漆的总附着量为基准。干燥后,第一层涂料的重量百分比为45-60 wt。%,优选为50-55 wt。%;版权:(C)2000,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号