摘要

In a first step, basic components including (A) 100 parts by weight of an organopolysiloxane gum, (B) 5-100 parts by weight of a reinforcing silica filler, and (C) 0.1-30 parts by weight of a processing aid are fed batchwise to a closed mixer for mixing them at a temperature of room temperature to 150° C. In a second step, the mixture is fed into a kneader/mixer for heat treating at a temperature of 150-250° C. The first step achieves quick dispersion and cooperates with the second step to form a heat-curable silicone rubber compound in an efficient manner.
机译:在第一步中,包含以下基本成分:(A)100重量份的有机聚硅氧烷胶,(B)5-100重量份的增强二氧化硅填料和(C)0.1-30重量份的加工助剂。分批进料到密闭的混合器中,以在室温至150℃下将它们混合。在第二步骤中,将混合物进料到捏合机/混合机中以在150-25℃的温度下进行热处理。 C.第一步实现快速分散,并与第二步配合以有效方式形成可热固化的硅橡胶混合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号