首页> 外国专利> A process for preparing Zeolite Catalysts with AIPO4 acids combined with catalytic activity and / or hydrothermal stability improvedA process for improving the catalytic activity and hydrothermal stability of Zeolite Catalysts, a process for Cracking Hydrocarbon with a

A process for preparing Zeolite Catalysts with AIPO4 acids combined with catalytic activity and / or hydrothermal stability improvedA process for improving the catalytic activity and hydrothermal stability of Zeolite Catalysts, a process for Cracking Hydrocarbon with a

机译:结合催化活性和/或水热稳定性改进了用AIPO4酸制备沸石催化剂的方法改进了沸石催化剂的催化活性和水热稳定性的方法

摘要

A process for preparing acidic Zeolite Catalysts of medium or small pores with AIPO4 combined with catalytic activity and / or hydrothermal unaestabilidad improvedA process for improving the catalytic activity or laestabilida D hydrothermal Zeolite Catalysts and Cracking process for Hydrocarbon with a catalyst and a Composition of matterIncludes Zeolite Catalysts prepared by or improved processes.The process to improve the catalytic Activ ity of a catalyst of acidic Zeolite pores or small media comprises the steps of treating lazeolita with a Phosphorus Compound to form a ZeWavelet and combine with Phosphorus treated Zeolite treated with AIPO4 confosforo. The option onalmente zeolitatratada with Phosphorus is Calcined.The stage of combining with AIPO4 Zeolite can optionally be followed by steaming The Catalyst combined.The fosforosutiles containing compounds for the treatment of Zeolite include Phosphoric Acid or Ammonium dihydrogen phosphate, mono, fosfitosorgu00e1nicos, and organofosfinas.The Phosphorus containing Compound is preferably an Ammonium acid phosphate.The process to increase estabilidadhidrotu00e9rmica a Zeolite Catalyst comprises First treating a Zeolite with a compound containing Phosphorus and then mix with AIPO4.The catalizadorasu00ed prepared may be used alone or combined with other Catalysts.Can also be used in a p roceso for Cracking hydrocarbons which comprises contacting a feed material to a Hydrocarbon Catalyst prepared as described aboveMind.
机译:一种具有AIPO4的中孔或小孔酸性沸石催化剂的制备方法,该方法结合了催化活性和/或水热不易变性改进了一种用于提高催化活性或可水解的D型水热沸石催化剂的方法以及用催化剂和物质组成的烃裂化方法包括通过改进方法制备的沸石催化剂。提高酸性沸石孔或小介质的催化剂的催化活性的方法包括用磷化合物处理lazeolita以形成ZeWavelet并与经AIPO4 Confosforo处理的经磷处理的沸石结合的步骤。 。煅烧含磷的onalmente zeolitatratada煅烧。可以在与AIPO4沸石合并的阶段中进行蒸汽蒸煮,然后组合催化剂。用于处理沸石的fosforosutiles化合物包括磷酸或磷酸二氢铵,单,fosfitosorg含磷的化合物优选是磷酸铵。增加稳定化沸石催化剂的方法包括首先用含磷的化合物处理沸石,然后与AIPO4混合。也可以用于裂解烃的方法中,该方法包括使进料与按上述方法制备的烃催化剂接触。

著录项

  • 公开/公告号AR014709A1

    专利类型

  • 公开/公告日2001-03-28

    原文格式PDF

  • 申请/专利权人 EXXON CHEMICAL PATENTS INC.;

    申请/专利号AR1999P101049

  • 发明设计人

    申请日1999-03-11

  • 分类号B01J29/90;B01J27/16;B01J29/06;C10G11/05;C10G11/18;

  • 国家 AR

  • 入库时间 2022-08-22 01:26:23