An Ni3Al-base heat-resistant alloy containing, in %by weight,6.0 to 9.0% of Al, 2.0 to 15.0% of Cr and 0.5 to3.0% of Zr, the balance being Ni and inevitable impurities,the alloy having a metal structure comprising Ni3Al as themain phase thereof. When required, the alloy may furthercontain over 0% to not more than 5.0% of W, over 0% to not morethan 3.0% of Mo, over 0% to not more than 3.0% of Nb, over 0%to not more than 0.003% of B, over 0% to not more than 0.3% ofC and 0.003 to 0.03% of N, wherein the combined amount of W, Moand Nb is up to 5.0% if at least two of these elements arepresent.
机译:Ni3Al基耐热合金,以%表示以重量计,铝为6.0至9.0%,铬为2.0至15.0%,0.5至0.5%Zr的3.0%,其余为Ni和不可避免的杂质,具有包括Ni3Al作为金属的金属结构的合金其主要阶段。如果需要,合金可能会进一步含有超过0%至不超过5.0%的W,超过0%至不超过Mo的3.0%以上,Nb的0%以上,Nb的3.0%以下以下不超过B的0.003%,不超过B的0%至不超过0.3%C和0.003-0.03%的N,其中W,Mo的总含量如果这些元素中的至少两个为Nb,则Nb最高为5.0%当下。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号