FIELD: manufacture of artificial glass fiber for industrial purposes. SUBSTANCE: artificial glass fibers having solubility at pH of 4.5, at least 20 nm daily, temperature along line of liquid of lower than 1300 C, viscosity at temperature along line of liquid of 300 P are manufactured from composition which comprises, wt %: SiO2, 36-55; Al2O3, 15-30; CaO, 3-30; MgO, 5-20, FeO, 4-15; Na2O+K2O, 1-15; TiO2, 0-6; other elements, 0-15 at Si4+ to Si4++Al3+ ratio less or equal to 0.67. Fibers are prepared in spinning bowl with holes or on cascade of spinning wheels. Package of said glass fibrous product contains indications on solubility at pH of 4 or 5 and/or in medium created by macrophages in lung liquid, and also solubility in vivo. EFFECT: fibers from inexpensive stock, resistant to weather conditions but having properties of biosolubility at pH of 4.5. 11 cl, 1 tbl
机译:领域:工业用人造玻璃纤维的制造。物质:由以下组成的人造玻璃纤维制成,该人造玻璃纤维在pH值为4.5时溶解度为每天至少20 nm,沿液体线的温度低于1300 C,沿温度线的粘度为300 P,该组合物包含以下成分:wt%:SiO 2 ,36-55; Al 2 O 3 ,15-30;氧化钙,3-30; MgO 5-20,FeO 4-15; Na 2 O + K 2 O,1-15; TiO 2 ,0-6;其他元素,Si 4 + 与Si 4 + + Al 3 + 的比值为0-15,小于或等于0.67。纤维在带孔的纺丝碗中或在级联的纺丝轮上制备。所述玻璃纤维产品的包装包含在pH为4或5时和/或在巨噬细胞在肺液中产生的培养基中的溶解度以及体内溶解度的指示。效果:来自廉价库存的纤维,具有耐候性,但在pH为4.5时具有生物溶解性。 11厘升,1汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号