首页> 外国专利> A method for Manufacturing a shaped Body containing a Starch, a homogenized Pulp containing Starch and a device for Manufacturing a Soft Capsule.

A method for Manufacturing a shaped Body containing a Starch, a homogenized Pulp containing Starch and a device for Manufacturing a Soft Capsule.

机译:一种用于制造包含淀粉的成形体的方法,一种包含淀粉的均质纸浆以及一种用于制造软胶囊的装置。

摘要

Method for Manufacturing a shaped Body containing Starch and a homogenized Pulp containing Starch and shaped bodies made of same. The method is carried out so that the value of viscosity Index constraint is made with the same mass of at least 40 ml / G.A limiting value of viscosity index ensures an elongation at the Breaking Point of the Extruded material of at least 150%, thanks to which it can produce Soft Capsules with capsule of a cover Piece, through the Rotary Swaging process.Claim 1: a method for Manufacturing a shaped Body containing Starch, in particular a Soft Capsule with a coverage of the capsule of a piece, which comprises the steps of: a) a mixture containing at least one Starch, preferably within a range of 45 80% by Weight with respect to the total weight of the mixture, Water Softener, and at least one OrganicWhen heated and mixed to give a Mass processable Thermoplastic in homogenized form, preferably in a First Processing device; (b) when it is appropriate to make an intermediate product that can be stored, in particular a GranulateAfter Cooling the mixture obtained in the Step a) and subsequently heating the intermediary product to give a Mass processable Thermoplastic in a Second Processing Device Manufacture; (c) at least one Coating material, in particular a film Extruded,The output of the first or where appropriate the second Processing device; (d) to reconvene the lining material in a Body formed by a continuous or intermittent Training Method; (e) where appropriate, dry the body shape,Where the steps (a) to (c) are carried out in such a way that in STEP (d), the Rate Limiting viscosity of starch in the Dough to form the coating material has a value not less than 40 ml / g, preferably of at least 50 ml / G and still more preferably by least 80 ml / G.
机译:包含淀粉的成形体和包含淀粉的均质纸浆的制造方法以及由其制成的成形体。进行该方法时,以相同的质量至少40 ml进行粘度指数约束的值/ GA粘度指数极限值可确保挤出材料的断裂点伸长率至少为150%,这要归功于权利要求1:一种用于制造包含淀粉的成型体的方法,特别是具有覆盖胶囊的胶囊的软胶囊,该软胶囊具有覆盖部件的胶囊,该方法包括:步骤:a)包含至少一种淀粉的混合物,优选相对于该混合物的总重量为45 80%重量范围内的淀粉,软水剂和至少一种有机物。均质形式的热塑性塑料,最好在第一加工设备中使用; (b)何时合适地制备可以储存的中间产物,特别是颗粒,将步骤a)中获得的混合物冷却后,随后加热该中间产物,以在第二加工装置制造中得到可大量加工的热塑性塑料; (c)至少一种涂料,特别是挤出的薄膜,第一或第二处理装置的输出; (d)将衬里材料重新放在通过连续或间歇训练方法形成的车身中; (e)在适当的情况下,干燥身体形状,其中步骤(a)至(c)的执行方式应使步骤(d)中面团中形成涂层材料的淀粉的限速粘度达到不小于40ml / g,优选至少50ml / g,还更优选至少80ml / g的值。

著录项

  • 公开/公告号AR035165A1

    专利类型

  • 公开/公告日2004-05-05

    原文格式PDF

  • 申请/专利权人 GREITHER PETER;

    申请/专利号AR2000P106063

  • 发明设计人

    申请日2000-11-16

  • 分类号A61K9/48;B01J13/00;

  • 国家 AR

  • 入库时间 2022-08-21 23:12:21

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号