PURPOSE: A production method of clinker and eco-cement using ash generated during the incineration of domestic waste and sewage sludge is provided, which recycles waste materials and saves energy due to low sintering temperature. CONSTITUTION: The clinker is produced by mixing 87-92wt.% of limestone, 1-4wt.% of alumina-based materials, 1-2wt.% of clay, 2-6wt.% of sewage sludge, 6-10wt.% of incineration ash, decarbonating the mixture at 900deg.C for 1hr and sintering it at 1250-1350deg.C for 1hr. Eco-cement is produced by grinding produced clinker to become powder having specific surface of 2000-6000cm¬2/g and adding 8-12wt.% of gypsum, preferably anhydrous gypsum obtained by heating gypsum selected from phosphogypsum byproduct, FGD gypsum, natural gypsum, etc. at 700-900deg.C.
机译:目的:提供一种使用焚烧生活垃圾和污水污泥产生的灰烬的熟料和生态水泥的生产方法,该方法可回收废物并由于烧结温度低而节省能源。组成:熟料是通过混合87-92wt。%的石灰石,1-4wt。%的氧化铝基材料,1-2wt。%的粘土,2-6wt。%的污水污泥,6-10wt。%的水泥焚烧灰分,将混合物在900°C脱碳1小时,然后在1250-1350°C烧结1小时。通过将生产的熟料研磨成比表面积为2000-6000cm2 / g的粉末,并加入8-12wt。%的石膏,优选通过加热选自磷石膏副产品,FGD石膏,天然石膏中的石膏而获得的无水石膏,来生产生态水泥。等温度为700-900摄氏度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号