METHOD FOR PRODUCING MATERIALS FOR CONSTRUCTION AND CIVIL ENGINEERING WORKS BY USING WASTE TIRES OR WASTE RUBBER MATERIALS AND THE PRODUCED MATERIALS FOR CIVIL ENGINEERING WORKS FORMED BY STICKING ON BRICKS, BOUNDARY STONES, AND PAVEMENT BRICKS

机译:通过使用废轮胎或废橡胶材料生产建筑和民用工程材料的方法以及通过在砖,边界石和路面砖上进行粘贴而形成的民用工程作品的材料

摘要

PURPOSE: A method for producing materials for construction and civil engineering works by using waste tires or waste rubber materials and the produced materials for civil engineering works are provided to absorb shock, to secure a water-proof function, to cut off an external environment condition, and to maximize the use span by the waste tires or waste rubber materials. CONSTITUTION: A method for producing materials(6) for construction and civil engineering works by using waste tires or waste rubber materials is composed of steps for sorting rubber chips of 0.3¯10mm by milling the waste tires or waste rubber materials with a crusher; making the mixture by inserting and agitating paints for showing colors and an adhesive agent in the selected rubber chips; and pressurizing and heating the mixture in a mold by a hydraulic press at the temperature of 140¯250 deg.C and sticking a molded material(2) made from the waste tires or waste rubber materials on pavement bricks(1) by an adhesive agent(5).
机译:目的:通过使用废轮胎或废橡胶材料来生产建筑和土木工程材料的方法,并且提供用于土木工程的材料以吸收冲击,确保防水功能,切断外部环境条件,并最大程度地减少了废轮胎或废橡胶材料的使用时间。组成:一种利用废旧轮胎或废旧橡胶材料生产建筑和土木工程材料的方法(6),该步骤包括以下步骤:用破碎机将废旧轮胎或废旧橡胶材料碾碎,将0.3×10mm的橡胶碎片分类;通过在选定的橡胶片中插入和搅拌油漆来显示颜色和粘合剂,从而制成混合物;用液压机在140℃至250℃的温度下对混合物中的混合物加压并加热,并用粘合剂将由废轮胎或废橡胶制成的模制材料(2)粘在路面砖(1)上(5)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号