FIELD: building materials industry; methods of production of the cement and the cement additive.;SUBSTANCE: the invention is pertaining to the field of building materials industry, in particular, to the method of production of the cement or the additive to the cement or to the concrete and may be used for production concrete and reinforced concrete at prefabricated, monolithic or prefabricated-monolithic house-building. The technical result of the invention is the increased milling capability, reduced power input and water consumption in production of the cement and the additive, the raised their quality. The above indicated purpose is realized by the method of production of the cement or the additive providing for crushing of the cement clinker and-or the additive in the roller-press mill with the subsequent grinding of the cement clinker and-or the additive in the tube mill. Before grinding exercise action by the alternating pulsing of the electromagnetic field intensity of 105-109 A/m and the pulse duration of(1-10)·10-2 s. At that the grinding in the roller-press mill is conducted up to the grade of particle - 100-1000 microns, and the subsequent grinding of the clinker and-or the additive conduct up to the size of particles of 10-80 microns. In the indicated method there may be used a tube mill with the diameter of 3.2 m and the length of 15 m with grinding balls sizing range: the 1st chamber - the balls with the diameter D - 70 mm and the mass of M - 17 t, D - 60 mm and the mass of M - 18 t, D - 50 mm and the mass of M - 15 t; the second chamber - the balls with the diameter D-30 mm and the mass of M - 80 t. The cement or the additive to the cement obtained by this method are characterized by the following grain contents (in mass %): 80 microns - 5.60 microns - 20, 50 microns - 20, 30 microns - 50, 10 microns - 5.;EFFECT: the invention ensures the increased milling capability, reduced power input and water consumption in production of the cement and the additive, the improved quality.;6 cl, 1 dwg
机译:领域:建材工业;水泥和水泥添加剂的生产方法。物质:本发明属于建筑材料工业领域,尤其涉及水泥或混凝土的水泥或添加剂的生产方法,并且可以是用于在预制,整体式或预制整体式房屋建筑中生产混凝土和钢筋混凝土。本发明的技术结果是提高了研磨能力,降低了水泥和添加剂生产中的功率输入和水消耗,提高了它们的质量。上述目的是通过生产用于粉碎水泥熟料和/或添加剂的方法来实现的,该方法是在辊压机中粉碎水泥熟料和/或添加剂,随后在水泥磨机中研磨水泥熟料和/或添加剂。管磨机。在磨削运动之前,通过交替脉冲以10 5 -10 9 A / m的电磁场强度和(1-10)&middot; 10 < Sup> -2 s。此时,在辊压机中进行的研磨达到颗粒级-100-1000微米,随后熟料和/或添加剂的研磨进行到粒径为10-80微米。在所示的方法中,可以使用直径为3.2 m,长度为15 m的管磨机,其研磨球的尺寸范围为:第一腔-直径D-70 mm的球,质量M-17 t ,D-60 mm,质量为M-18 t,D-50 mm,质量为M-15 t;第二个腔室-直径为D-30毫米,质量为M-80吨的球。通过该方法获得的水泥或水泥添加剂的特征在于以下晶粒含量(质量%):80微米-5.60微米-20、50微米-20、30微米-50、10微米-5。 :本发明确保了增加的研磨能力,减少了水泥和添加剂的生产中的功率输入和水消耗,提高了质量。; 6cl,1dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号