首页> 外国专利> METHOD OF PRODUCTION OF THE RAW MIXTURE FOR MANUFACTURE OF THE FINISHING AND ORNAMENTAL CONSTRUCTION PRODUCTS (VERSIONS)

METHOD OF PRODUCTION OF THE RAW MIXTURE FOR MANUFACTURE OF THE FINISHING AND ORNAMENTAL CONSTRUCTION PRODUCTS (VERSIONS)

机译:用于装饰和装饰建筑产品(版本)制造的原始混合物的生产方法

摘要

FIELD: construction industry; methods of production of the raw mixture for manufacture of the finishing and ornamental construction products.;SUBSTANCE: the invention is pertaining to the methods of production of the raw mixture for manufacture of the finishing and ornamental construction products. The technical result of the invention is manufacture the finishing and ornamental products having the balneologic effect with the heightened emission of the aeroions of an iodine, magnesium and bromine during the long period of time of operation and at keeping the basic operational performances - such as the strength and crack-resistance. The method of production of the raw mixture for manufacture of the finishing and ornamental products includes intermixing the caustic magnesite with the sawdust, with the subsequent dampening of the mass with the bischofite water solution, the final intermixing. At that the mixture is introduced with iodinolum with amount of 0.3-0.6 volumetric shares, which is beforehand stirred with the water solution of bischofite. The alternative version of the method includes intermixing of the caustic magnesite with the sawdust and the subsequent dampening of the mass with the bischofite water solution and the final intermixing. At that the mixture is added with the crystals of the carnallite mineral of 2 mm to 10 mm size in the amount of 0.25-0.4 vol. shares. The crystals of the carnallite mineral are added right after the final intermixing of the basic components of the mixture, and stir during no more than 1.5 minutes.;EFFECT: the invention ensures manufacture the finishing and ornamental products having the balneologic effect with the heightened emission of the aeroions of an iodine, magnesium and bromine during the long period of operation and at keeping the basic operational performances - such as the strength and crack-resistance.;3 cl, 1 tbl
机译:领域:建筑业;用于生产用于装饰和装饰建筑产品的原料混合物的方法。物质:本发明涉及用于制造用于装饰和装饰建筑产品的原料混合物的方法。本发明的技术结果是制造具有药理作用的整理和装饰产品,其在长时间的操作中碘,镁和溴的气态离子的排放增加,并且保持基本的操作性能,例如强度和抗裂性。生产用于制造精加工和装饰产品的原始混合物的方法包括将苛性菱镁矿与木屑混合,随后用重水铁矿水溶液润湿物料,最后进行混合。此时,将混合物与碘化物以0.3-0.6体积份的量引入,该碘化物事先与重水铁矿的水溶液一起搅拌。该方法的替代形式包括将苛性菱镁矿与锯末混合,然后用重水铁矿水溶液润湿物料并进行最终混合。此时,以0.25-0.4体积%的量添加2mm至10mm大小的角砾石矿物的晶体的混合物。分享。在混合物的基本成分最终混合后,立即添加角绿岩矿物的晶体,并在不超过1.5分钟的时间内搅拌。在长期运行过程中保持碘,镁和溴的气态并保持基本的运行性能-如强度和抗裂性; 3 cl,1 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com