Rotating anode plate producing method, involves forming base plate sleeve to net shape of anode plate, such that deformation degree to be realized in area of ring shaped tungsten-rhenium-alloy layer is larger than certain percentages
Rotating anode plate producing method, involves forming base plate sleeve to net shape of anode plate, such that deformation degree to be realized in area of ring shaped tungsten-rhenium-alloy layer is larger than certain percentages
The method involves forming a base plate sleeve (1) to a net shape of a rotating anode plate. A deformation degree to be realized in an area of a ring shaped tungsten-rhenium-alloy layer (3) is larger than 10 percentages, preferably 30 percentages. The anode plate is recrystallisation-annealed at an annealing temperature above 1500 degrees Celsius, preferably 1700 degrees Celsius over a period of 1 hour, preferably 4 hours.