MATERIAL FOR OPENING CRITERIA FOR PAINTING, MANUFACTURING AND OPENING CRITERIA AND PAINTING CRITERIA

机译:用于绘画,制造,绘画和绘画的开放标准的材料

摘要

A purpose of the present invention is to provide material of an aperture grille used for a color picture tube having excellent yield strength, excellent high temperature creep strength and excellent magnetic characteristic, material of an aperture grille used for a color picture tube for improving an occurrence of cracking during a hot rolling step, a method for producing these material, an aperture grille and a color picture tube with the aperture grille. After adding nickel of 0.01 to 1.75 wt% to low carbon alloy steel including copper of 0.05 to 2.5 wt% and phosphor of 0.001 to 0.4 wt%, material according to the present invention is cold rolled. Then, a precipitation treatment is processed at a temperature of 300 to 700 DEG C. Alternatively, the material is cold rolled and secondary rolled after passing through an intermediate annealing at a temperature of 500 to 800 DEG C. Then, the precipitation treatment is processed.
机译:本发明的目的是提供一种具有优异的屈服强度,优异的高温蠕变强度和优异的磁特性的用于彩色显像管的格栅的材料,用于改善发生率的用于彩色显像管的格栅的材料。热轧步骤中产生裂纹的方法,生产这些材料的方法,孔栅和具有孔栅的彩色显像管。向包含0.05至2.5重量%的铜和0.001至0.4重量%的磷的低碳合金钢中添加0.01至1.75重量%的镍之后,将根据本发明的材料冷轧。然后,在300至700℃的温度下进行沉淀处理。或者,将材料在500至800℃的温度下经过中间退火后,进行冷轧和二次轧制。然后,进行沉淀处理。 。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号