PROCESS FOR MAKING IMPROVED HIGH ALUMINA REFRACTORY CEMENT CONTAINING MG-AL SPINEL FROM DOLOMITE.

机译:用白云石制作含有MG-AL尖晶石的改良型高铝耐火水泥的方法。

摘要

The present invention relates to the process for developing high alumina refractory cement comprising spinel phase and the said spinel phase comprises magnesia and alumina from dolomite and calcined alumina source. The said process comprises steps like selection of viable compositions comprising suitable percentages of dolomite containing cementing phases, preparation of refractory cement samples from said compositions for treating of cementing properties, characterization and optimization of different phases of refractory cement based on X-ray diffraction properties and identification and formation of high alumina refractory cement comprising 30 to 35 % spinel phase.
机译:本发明涉及用于开发包含尖晶石相的高氧化铝耐火水泥的方法,所述尖晶石相包括来自白云石和煅烧氧化铝源的氧化镁和氧化铝。所述方法包括以下步骤:选择包含合适百分比的含白云石的固相的可行组合物,从所述组合物中制备用于处理胶凝性能的耐火水泥样品,基于X射线衍射性能表征和优化耐火水泥的不同相。鉴定和形成包含30%至35%尖晶石​​相的高铝质耐火水泥。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号