Methods for making stretch shirting fabric having fabric weight less than 175 g/mSUP2 /SUPand fabric stretch between 15% to 45% in the weft direction are disclosed. A corespun composite elastomeric yarn is produced either (a) by low draft (2.7x or below) core-spinning of the elastomeric yarn, or (b) by pretreating the corespun composite yarn in steam or heated water at temperatures of at least 110° C. to reduce yarn power before dyeing or weaving. The shirting fabric with such corespun composite elastomeric yarn in the weft meets end-use specifications without heat-setting.
展开▼
机译:公开了一种用于制备织物重量小于175g / m 2且在纬纱方向上拉伸率在15%至45%之间的拉伸衬衫织物的方法。包芯复合弹性纱是通过(a)通过低牵伸度(2.7x或更低)的芯纱纺丝生产的;或(b)通过在蒸汽或热水中于至少110°C的温度下对包芯复合纱进行预处理而制成的C.在染色或编织之前降低纱线强度。在纬纱中具有这种包芯复合弹性体纱线的衬衫面料满足最终使用规范,而无需热定形。