The present invention provides a method of producing polyalkylene terephthalate, which comprises: introducing a prepolymer of polyalkylene terephthalate that is in a molten state comprising 70 mol% or more of ethylene terephthalate or 1,4-butylene terephthalate repeating units and having an intrinsic viscosity [η] between 0.2 and 2 dl/g through a feed opening to a polymerization reactor; discharging the introduced prepolymer from holes of a perforated plate; and polymerizing the prepolymer under reduced pressure, while allowing the prepolymer to fall along the surface of a support that is open towards the outside at a temperature between the [crystalline melting point - 10°C] of the prepolymer or higher and the [crystalline melting point + 30°C] of the prepolymer or lower under the conditions represented by a formula S1/S2 1, wherein S1 is the surface area of falling polyalkylene terephthalate, and S2 is the area where the support is in contact with polyalkylene terephthalate.
机译:本发明提供了一种生产聚对苯二甲酸亚烷基酯的方法,该方法包括:引入处于熔融状态的聚对苯二甲酸亚烷基酯的预聚物,该预聚物包含70摩尔%或更多的对苯二甲酸乙二酯或1,4-对苯二甲酸丁二酯重复单元并具有特性粘度[ η]通过聚合反应器的进料口在0.2和2 dl / g之间;从多孔板的孔中排出引入的预聚物;在减压下聚合该预聚物,同时使该预聚物在预聚物的[结晶熔点-10℃]或更高与[结晶熔体]之间的温度下沿着向外部敞开的载体的表面下落。在由式S1 / S2> 1表示的条件下,预聚物的熔点为+ 30℃或更低;其中S1为下落的聚对苯二甲酸亚烷基酯的表面积,S2为载体与聚对苯二甲酸亚烷基酯接触的面积。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号