SIMPLIFIED METHOD OF ROLLED PRODUCTS MANUFACTURE OF Al-Zn-Mg ALLOYS, AND PRODUCTS MANUFACTURED USING THIS METHOD

机译:Al-Zn-Mg合金轧制产品制造的简化方法以及使用该方法制造的产品

摘要

FIELD: metallurgy.;SUBSTANCE: said utility invention relates to Al-Zn-Mg alloys, namely, to alloys for welded structures, such as structures used in marine construction, during manufacture of car and industrial vehicle bodies, and stationary or movable tanks. The method involves manufacture of a plate using semi-continuous casting. The plate is made of an alloy containing, % weight: Mg 0.5-2.0, Mn 1.0, Zn 3.0-9.0, Si 0.50, Fe 0.50, Cu 0.50, Ti 0.15, Zr 0.20, Cr 0.50, aluminium with its inevitable impurities being the remaining, Zn/Mg 1.7. After that, the plate is subjected to homogenisation and/or reheating at a temperature T1 selected so that 500°C ≤T1≤(Ts-20°C) where Ts is the alloy burning temperature. The first hot rolling stage includes one or several rolling passes on a hot-rolling mill, the input temperature T2 is selected so that (T1-60°C)≤T2≤ (T1-5°C), and the rolling process is performed in such a way that the output final temperature T3 would be so that (T1-150°C)≤T3≤(T1-30°C) and T3 T2. The strip produced at the said first hot rolling stage is rapidly cooled to the temperature T4. The second stage of hot rolling of the said strip is performed at the input temperature T5 selected so that T5≤T4 and 200°C≤T5≤300°C. The rolling process is performed in such a way that the coiling temperature T6 would be so that (T5-150°C)≤T6≤(T5-20°C).;EFFECT: enhancement of balance between mechanical properties and corrosion resistance of base metal and welded joint using simplest and most reliable method.;34 cl, 8 dwg, 20 tbl, 10 ex
机译:发明领域本实用新型涉及Al-Zn-Mg合金,即涉及用于在汽车和工业车辆的车身的制造过程中以及在固定或可移动的储罐中用于焊接结构的合金,例如用于海事建筑的结构。该方法包括使用半连续铸造制造板。该板由以下合金制成:%Mg 0.5-2.0,Mn <1.0,Zn 3.0-9.0,Si <0.50,Fe <0.50,Cu <0.50,Ti <0.15,Zr <0.20,Cr <0.50,铝,残留不可避免的杂质,Zn / Mg> 1.7。之后,将板在选择的温度T 1 下进行均质化和/或再加热,以使温度为500℃& T 1 &le;(T s -20℃),其中T s 是合金燃烧温度。第一热轧阶段包括在热轧机上进行一次或多次轧制,选择输入温度T 2 ,使(T 1 -60°C)&le ; T 2 &le; (T 1 -5℃),并且以使得输出最终温度T 3 为(T 1 -150&deg; C)&le; T 3 &le;(T 1 -30°C)和T 3 2 。在所述第一热轧阶段生产的带钢被迅速冷却至温度T 4 。所述带材的热轧的第二阶段在选择的输入温度T 5 下进行,以使T 5 &le; T 4 和200° ; C&le; T 5 &le; 300℃。轧制过程以使卷取温度T 6 为(T 5 -1500℃] T 6 的方式进行。 Sub>&le;(T 5 -20°C)。效果:使用最简单,最可靠的方法增强母材和焊接接头的力学性能和耐腐蚀性之间的平衡。; 34 cl,8 dwg,20汤匙,10前

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号