To form a chromium oxide film on the inner surface of a Cr containing nickel-base alloy tube inexpensively and uniformly, the Cr containing nickel-base alloy tube is heated in atmospheric gas of carbon dioxide gas and non-oxidation gas to form an oxide film consisting of chromium oxide having a thickness of 0.2 to 1.5 μm on the inner surface of the Cr containing nickel-base alloy tube. The atmospheric gas may contain oxygen gas of 5 vol % or less and/or water vapor of 7.5 vol % or less.
机译:为了廉价且均匀地在含Cr的镍基合金管的内表面上形成氧化铬膜,将含Cr的镍基合金管在二氧化碳气体和非氧化性气体的大气中加热以形成氧化膜。在含Cr的镍基合金管的内表面上由厚度为0.2至1.5μm的氧化铬构成。大气气体可包含5体积%以下的氧气和/或7.5体积%以下的水蒸气。