PROBLEM TO BE SOLVED: To provide a prediction method of a neutralization depth of concrete subjected to application of a finishing coating material.;SOLUTION: A neutralization resistance value R of the finishing coating material is determined from formula (2), by using a thickness d and a CO2 diffusion coefficient Df of the finishing coating material acquired from measurement relative to the finishing coating material, and the neutralization depth x is predicted from formula (1), where A is the neutralization speed coefficient of concrete (known), t is material age, and Dc is the CO2 diffusion coefficient of the concrete (known).;COPYRIGHT: (C)2010,JPO&INPIT
展开▼
机译:要解决的问题:提供一种预测施加面漆的混凝土中和深度的方法。解决方案:面漆的中和电阻值R由公式(2)通过使用厚度确定d和通过测量获得的整理涂料相对于整理涂料的CO 2 Sub>扩散系数D f Sub>,并且根据公式(1)预测中和深度x ,其中A是混凝土的中和速度系数(已知),t是材料年龄,D c Sub>是混凝土的CO 2 Sub>扩散系数(已知)。版权:(C)2010,日本特许厅和INPIT