In a method of producing a strip suitable for further processing to yield a(110)[001] grain oriented electrical steel from a thin strip such as acontinuously cast thin strip the thin cast strip is processed to promoterecrystallization from the surface layer of the strip (S=0) into the quarterthickness of the strip (S=0.2 to 0.3). The process parameters are selected sothat the strain/recrystallization parameter (K*)-1, =about 6500 and wherein,Formula (I), THBA is the annealing temperature of the strip (in ~Kelvin), THRis the hot rolling temperature of the strip (in ~Kelvin), .epsilon. is thestrain rate of hot rolling, ti is the initial thickness of the strip beforehot rolling, and tf is the final thickness of the strip after hot rolling.
机译:在一种生产条带的方法中,该条带适于进一步加工以产生(110)[001]薄带等方向性电磁钢连铸薄带薄铸带经过处理以促进从带材表面层(S = 0)再结晶到四分之一条的厚度(S = 0.2至0.3)。选择工艺参数是为了应变/再结晶参数(K *)-1,> =约6500,其中,式(I),THBA是带材的退火温度(以开尔文为单位),THR是带材的热轧温度(以开尔文为单位),ε。是个热轧的应变率,ti是带材之前的初始厚度tf是热轧后带钢的最终厚度。

著录项

  • 公开/公告号CA2459479C

    专利类型

  • 公开/公告日2010-06-01

    原文格式PDF

  • 申请/专利权人 AK STEEL PROPERTIES INC.;

    申请/专利号CA20022459479

  • 发明设计人 HUPPI GLENN S.;SCHOEN JERRY W.;

    申请日2002-09-13

  • 分类号C21D8/12;C21D9/52;

  • 国家 CA

  • 入库时间 2022-08-21 18:42:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号