FIELD: construction.;SUBSTANCE: method for production of portland cement includes production of portland cement clinker, containing tricalcium silicate, bicalcium silicate, tricalcium aluminate and four-calcium alumoferrite, sintering of initial cement raw mix, containing calcium, silica-alumina, ferriferous components and fluorine-containing mineralisator - fluorine-carbon-containing wastes of electrolytic production of aluminium in amount of 0.1-0.25 wt % as equivalent to fluorine from initial raw mix, cooling and grinding of clinker with gypsum. According to another version of invention, fluorine-containing mineralisator is represented by mixture of fluorite and above-specified wastes at their following content, wt % as equivalent to fluorine: specified wastes - 0.1-0.2, fluorite - the rest till content of fluorine in raw mix of 0.15-0.4 wt %. Specified wastes are represented by dust of electric filters or sludge of gas treatment, or flotation tailings of coal froth.;EFFECT: reduced specific consumption of fuel for clinker annealing, improved efficiency and prolonged overhaul life of furnace, efficiency of mills operation in process of clinker grinding, recycling of aluminium production wastes.;8 cl, 27 tbl, 5 ex
机译:领域:建筑;物质:硅酸盐水泥的生产方法包括硅酸盐水泥熟料的生产,该硅酸盐水泥包含硅酸三钙,硅酸二钙,铝酸三钙和四钙铝铁矿,烧结初始水泥生料,包含钙,硅铝,铁酸盐成分和含氟矿化剂-铝的电解生产中含氟碳废料的量相当于最初原料混合物中氟的0.1-0.25 wt%,冷却和熟料与石膏的研磨。根据本发明的另一种形式,含氟矿化剂由萤石和以上指定废物的混合物组成,其含量如下:相当于氟的wt%:指定废物-0.1-0.2,萤石-其余的直到氟的含量。 0.15-0.4重量%的原料混合物。特定的废物以电过滤器的粉尘或气体处理的污泥或泡沫浮选尾渣为代表;效果:减少了熟料退火的燃料比消耗,提高了效率并延长了炉子的大修寿命,工厂在运行过程中的运转效率熟料磨,铝生产废料的回收。; 8 cl,27 tbl,5 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号