PROCEDURE FOR APPLICATION OF SLAG SCULL ON CONVERTER LINING

机译:渣SC在变流器内衬上的应用程序

摘要

FIELD: metallurgy.;SUBSTANCE: disclosed here procedure refers to ferrous metallurgy, particularly to procedures of hot repair of lining of steel melting aggregates. The procedure consists in turn-down of the converter and in tapping metal subjected to oxidising blow-off, in leaving slag of preceding melt in the converter, in introducing carbonate materials and carbon containing fuel, in applying it on internal walls of the converter by means of supplying jets of neutral gas from top via a tuyere from an alternate height above the level of a quiet bath. Prior to and/or in the period of supplying jets of neutral gas from above on residual slag dolomite, carbon containing fuel and lime are introduced as carbonate materials and carbon containing fuel at ratio 1:(0.2-0.6):(0.4-0.6) correspondingly. Supply of neutral gas in the first period of 10-30 sec is performed at consumption rate 20-25m3/min·per t of retained slag of the preceding melt via the tuyere positioned at height of correspondingly 15-30 reduced calibres of tuyere nozzle diametre above the level of a quiet bath. Further, height of the tuyere is lowered to 7-12 reduced calibres of diametre of its nozzle. During 5…25 sec height of the tuyere is successively changed within the range 7-30 of reduced calibres of diametre of its nozzle. Consumption of neutral gas is maintained equal to 1.1-1.5 of consumption of gas of the first period.;EFFECT: increased efficiency of slag scull application on lining of converter.;3 ex
机译:技术领域:冶金学;物质:在此公开的方法是指黑色冶金,特别是指对钢水熔融集料的衬里进行热修复的方法。该程序包括:关闭转炉,放出经过氧化吹脱的金属,将先有熔体的炉渣留在转炉中,引入碳酸盐材料和含碳燃料,然后将其施加到转炉内壁上。通过静水槽上方另一高度的风口从顶部供应中性气体的装置。在从上方向残留矿渣白云石上供应中性气体射流之前和/或期间,将含碳燃料和石灰作为碳酸盐材料引入,含碳燃料的比例为1:(0.2-0.6):( 0.4-0.6)相应地。在第一个10-30秒的时间内,通过消耗风口的进料速度为20-25m 3 / min·t的方式,通过位于相应高度15的风口来供应中性气体。将风口喷嘴直径的-30口径降低到安静浴池上方的水平。此外,将风口的高度降低至其喷嘴直径的减小的7-12口径。在5…25秒内,风口的高度在其喷嘴直径减小的口径的7-30范围内连续变化。中性气体的消耗量保持等于第一时期的气体消耗量的1.1-1.5。效果:提高转炉炉衬衬渣的效率。3ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号