PURPOSE: Glass frit for an unleaded sealant, a filler using thereof, and a crystallinity increasing method of the filler are provided to offer the environmentally-friendly property to a binder or the sealant for an electronic component or a display. CONSTITUTION: Glass frit for an unleaded sealant capable of low-temperature sintering and heat-treating at the temperature lower than 430deg C contains the following: a main composition containing 1.5mol of SnO2, 0.9mol of P2O5, and 0.05mol of Al2O3; and 0.1mol of more than two compounds selected from ZnO, Li2O, TiO2, ZrO2, or CaO. The main component additionally contains 0.1mol of B2O3.
机译:用途:提供无铅密封剂用玻璃粉,使用其的填料以及填料的结晶度提高方法,以为粘合剂或电子部件或显示器用密封剂提供环保特性。组成:能够在低于430摄氏度的温度下进行低温烧结和热处理的无铅密封剂玻璃粉,其主要成分如下:主要成分为1.5摩尔的SnO2、0.9摩尔的P2O5和0.05摩尔的Al2O3; 0.1mol的选自ZnO,Li2O,TiO2,ZrO2或CaO的两种以上化合物。主要成分还包含0.1摩尔的B2O3。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号