机译:丙烯酸树脂溶液,丙烯酸压敏胶粘剂,丙烯酸压敏胶粘剂,用于光学元件的丙烯酸压敏胶粘剂,带有压敏胶粘剂层的光学元件以及制备丙烯酸树脂的方法

摘要

PROBLEM TO BE SOLVED: To provide a solution-based acrylic pressure-sensitive adhesive of a bridge agent curable type, which enables heavy-thickness coating and can obtain a heavy-thickness pressure-sensitive adhesive layer.SOLUTION: This acrylic resin solution contains an acrylic resin (A) obtained by polymerizing a monomer component (a) containing a (meth)acrylic acid alkyl ester-based monomer as a main component under the existence of an organic solution (b) whose chain transfer constant to the organic solution of a vinyl acetate at a temperature of 60°C is not smaller than 250. The weight average molar weight of the acrylic resin (A) is 50,000 to 300,000, and a solid content concentration of the resin solution is not lower than 60%.
机译:解决的问题:提供桥剂固化型的溶液型丙烯酸类压敏胶粘剂,该胶粘剂能够进行厚膜涂布并获得厚膜压敏胶粘剂层。在有机溶液(b)的存在下,通过将包含(甲基)丙烯酸烷基酯基单体的单体组分(a)聚合为主要组分而得到的丙烯酸树脂(A),该有机溶液的链转移常数对a的有机溶液在60℃的温度下乙酸乙烯酯为250以上。丙烯酸树脂(A)的重均摩尔质量为50,000〜300,000,树脂溶液的固体成分浓度为60%以上。

著录项

  • 公开/公告号JP2012021142A

    专利类型

  • 公开/公告日2012-02-02

    原文格式PDF

  • 申请/专利权人 NIPPON SYNTHETIC CHEM IND CO LTD:THE;

    申请/专利号JP20110117251

  • 发明设计人 YAMABAYASHI AKIRA;

    申请日2011-05-25

  • 分类号C08F2/06;C09J133/06;C09J7/02;C08F20/10;C08L33/04;

  • 国家 JP

  • 入库时间 2022-08-21 17:41:39

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号