PROBLEM TO BE SOLVED: To provide a method for forming a fluorinated passive film capable of forming a fluorinated passive film having corrosion resistance on an iron steel base material other than a stainless steel material.;SOLUTION: The method for forming a fluorinated passive film is characterized in that a base material made of carbon steel or special steel (other than stainless steel) is subjected to baking, and is then subjected to fluorination treatment at 50 to 150°C.;COPYRIGHT: (C)2008,JPO&INPIT
机译:解决的问题:提供一种形成氟化钝化膜的方法,该方法能够在除不锈钢材料之外的铁钢基材上形成具有耐蚀性的氟化钝化膜。其特征在于,对碳素钢或特殊钢(除不锈钢以外)制成的基材进行烘烤,然后在50至<150℃下进行氟化处理。版权所有:(C)2008,JPO&INPIT

著录项

  • 公开/公告号JP4912163B2

    专利类型

  • 公开/公告日2012-04-11

    原文格式PDF

  • 申请/专利权人 ステラケミファ株式会社;

    申请/专利号JP20070004788

  • 发明设计人 里永 知彦;山田 宗孝;

    申请日2007-01-12

  • 分类号C23C8/08;C22C38/00;C22C38/04;C22C38/36;

  • 国家 JP

  • 入库时间 2022-08-21 17:39:04

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号