首页> 外国专利> COMPOSITION OF SULPHATE RESISTANCE POLYMER REPAIR MORTAR

COMPOSITION OF SULPHATE RESISTANCE POLYMER REPAIR MORTAR

机译:耐硫酸盐聚合物修补砂浆的组成

摘要

PURPOSE: A sulfate-resistant polymer-repairing mortar composition is provided to suppress the abrasion of rebar and the generation of surface cracks on concrete due to sulfate by using granulated slag powder and air-cooled slag powder. CONSTITUTION: A sulfate-resistant polymer-repairing mortar composition includes 80-85 weight% of granulated slag powder, 6-13 weight% of gypsum, 3-8 weight% of lime, normal cement, sodium sulfuric acid or potassium sulfuric acid, and air-cooled slag powder. The contents of the normal cement, the sodium sulfuric acid or the potassium sulfuric acid, and air-cooled slag powder are respectively more than 0 weight% and are less than or equal to 2 weight%. Sulfate-resistant polymer-repairing mortar includes 43-55 weight% of sulfate-resistant cement, 38-53 weight% of silica, reinforcing fiber, silicon-based antifoaming agent, redispersion acryl powder, and a wetting agent. The contents of the silicon-based antifoaming agent and the wetting agent are respectively more than 0 weight% and are less than or equal to 1 weight%. The content of the redispersion acryl powder is more than 0 weight% and is less than or equal to 3 weight%.
机译:用途:提供耐硫酸盐聚合物修补砂浆组合物,以通过使用粒状矿渣粉和风冷矿渣粉来抑制钢筋的磨损和由于硫酸盐而在混凝土上产生的表面裂缝。组成:耐硫酸盐聚合物修补砂浆组合物,包括80-85重量%的粒状矿渣粉,6-13重量%的石膏,3-8重量%的石灰,普通水泥,硫酸钠或硫酸钾,以及风冷渣粉。普通水泥,硫酸钠或硫酸钾,以及风冷渣粉的含量分别大于0重量%且小于或等于2重量%。耐硫酸盐聚合物修补砂浆包括43-55重量%的耐硫酸盐水泥,38-53重量%的二氧化硅,增强纤维,硅基消泡剂,丙烯酸再分散粉和润湿剂。硅基消泡剂和湿润剂的含量分别大于0重量%且小于或等于1重量%。再分散丙烯酸酯粉末的含量大于0重量%且小于或等于3重量%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号