首页> 外国专利> METHOD FOR MANUFACTURING STERILIZING ZEOLITE USING A WASTE RESID FLUIDIZED CATALYTIC CRACKING CATALYST CAPABLE OF SAVING COSTS REQUIRED FOR RAW MATERIALS BY RECYCLING THE WASTE RESID FLUIDIZED CATALYTIC CRACKING CATALYST

METHOD FOR MANUFACTURING STERILIZING ZEOLITE USING A WASTE RESID FLUIDIZED CATALYTIC CRACKING CATALYST CAPABLE OF SAVING COSTS REQUIRED FOR RAW MATERIALS BY RECYCLING THE WASTE RESID FLUIDIZED CATALYTIC CRACKING CATALYST

机译:利用废渣流态催化裂化催化剂的再生能力,利用废渣的流态催化裂化催化剂制造沸石的方法

摘要

PURPOSE: A method for manufacturing sterilizing zeolite using a waste resid fluidized catalytic cracking(RFCC) catalyst is provided to stably supply raw materials to a zeolite manufacturing process.;CONSTITUTION: Waste RFCC is directly ion-exchanged or is ion-exchanged after oxidization. The waste RFCC is composed of 60-70% of silicon dioxide, 25-32% of aluminum oxide, 0.1-0.5% of iron, 0.1-0.4% of nickel, and 0.1-0.4% of vanadium. The waste RFCC is generated from the oil petroleum refining process of a petrochemical industry. A filtering process, a washing process, a drying process, and a grinding process are implemented after the ion-exchanging process. A vibration mill and a centrifugal-vibration mill are used for the grinding process. Copper sulfate and ammonium nitrate are used for the ion-exchanging process.;COPYRIGHT KIPO 2012
机译:目的:提供一种利用废渣流化催化裂化(RFCC)催化剂生产灭菌沸石的方法,以稳定地向沸石生产过程中提供原材料。废RFCC由60-70%的二氧化硅,25-32%的氧化铝,0.1-0.5%的铁,0.1-0.4%的镍和0.1-0.4%的钒组成。废RFCC是从石化行业的石油石油精炼过程中产生的。在离子交换过程之后实施过滤过程,洗涤过程,干燥过程和研磨过程。研磨过程使用振动磨和离心振动磨。硫酸铜和硝酸铵用于离子交换过程。; COPYRIGHT KIPO 2012

著录项

  • 公开/公告号KR20120062068A

    专利类型

  • 公开/公告日2012-06-14

    原文格式PDF

  • 申请/专利权人 MUN HYUNG MO;KIM MYUNG SUN;

    申请/专利号KR20100123158

  • 发明设计人 KIM MYUNG SUN;KIM SAE HAN;

    申请日2010-12-06

  • 分类号C01B39/02;B09B3;B02C19/16;A01N59/16;

  • 国家 KR

  • 入库时间 2022-08-21 17:09:48

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号