PURPOSE: A wool fiber with soft texture and a method for fabricating the same are provided to split the wool fiber in a longitudinal direction and to enhance soft texture.;CONSTITUTION: A method for fabricating a wool fiber comprises a step of treating the wool fibers with high temperature acidic solution and ultrasonic wave and a step of partially splitting the wool fiber in a longitudinal direction. The wool fiber contains cuticle layer-removed cortex and cell membrane complex. The average end fineness and fiber length of the wool fiber is 5-10 um and 40-65 mm. The acidic solution is a formic acid solution. A method for fabricating a wool fabric comprises: a step of dyeing the wool fiber; a step of spinning the fiber to prepare a grey yarn; a step of weaving the grey yarn to prepare a fabric; and a step of processing the fabric.;COPYRIGHT KIPO 2013
机译:目的:提供一种具有柔软质地的羊毛纤维及其制造方法,以在纵向方向上将羊毛纤维分开并增强柔软质地。;构成:一种制造羊毛纤维的方法包括处理羊毛纤维的步骤用高温酸性溶液和超声波处理,以及将羊毛纤维在纵向上部分分裂的步骤。羊毛纤维包含去除表皮层的皮质和细胞膜复合物。羊毛纤维的平均末端纤度和纤维长度为5-10微米和40-65毫米。酸性溶液是甲酸溶液。一种羊毛织物的制造方法,包括:将羊毛纤维染色的步骤;以及将羊毛纤维染色的步骤。将纤维纺丝以制备坯纱的步骤;编织坯纱以制备织物的步骤;以及面料的加工步骤。; COPYRIGHT KIPO 2013

著录项

  • 公开/公告号KR20120125681A

    专利类型

  • 公开/公告日2012-11-19

    原文格式PDF

  • 申请/专利权人 CHEIL INDUSTRIES INC.;

    申请/专利号KR20110043273

  • 发明设计人 OH WON SEOK;JEONG JAE SEOK;DO UK HO;

    申请日2011-05-09

  • 分类号D01C3/00;D02J1/18;D01B9/00;

  • 国家 KR

  • 入库时间 2022-08-21 16:28:43

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号