PURPOSE: A method for manufacturing extruded aluminum alloy is provided to homogenize an aluminum alloy billet by preheating the aluminum alloy billet at high temperature.;CONSTITUTION: A method for manufacturing extruded aluminum alloy is as follows; a step for generating an aluminum alloy billet by injecting molten steel in a mold(S10); a step for cutting the aluminum alloy billet at a constant size(S20); a step for homogenizing micro segregation(S30); a step for chamfering the surface of the aluminum alloy billet(S40); and a step for extruding the aluminum alloy billet to a desired shape(S50).;COPYRIGHT KIPO 2013;[Reference numerals] (S10) Casting step; (S20) Cutting step; (S30) Heating step; (S40) Chamfering step; (S50) Extruding step
机译:目的:提供一种挤压铝合金的制造方法,通过在高温下对铝合金坯进行预热来使铝合金坯均质化。组成:挤压铝合金的制造方法如下;通过在模具中注入钢水产生铝合金坯料的步骤(S10);以恒定尺寸切割铝合金坯料的步骤(S20);使微偏析均质化的步骤(S30);对铝合金坯的表面进行倒角的步骤(S40); COPYRIGHT KIPO 2013; [附图标记](S10)铸造步骤;以及将铝合金坯料挤压成所需形状的步骤(S50)。 (S20)切割步骤; (S30)加热步骤; (S40)倒角步骤; (S50)挤出步骤

著录项

  • 公开/公告号KR20130029965A

    专利类型

  • 公开/公告日2013-03-26

    原文格式PDF

  • 申请/专利权人 DAE YEONG METAL CO. LTD.;

    申请/专利号KR20110093420

  • 申请日2011-09-16

  • 分类号B21C23/00;C22F1/04;B22D21/04;

  • 国家 KR

  • 入库时间 2022-08-21 16:27:28

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号