PURPOSE: A method for manufacturing colored aluminum product without degrading chromaticity or colored aluminum alloy product, color composition for coloring and the colored aluminum product, or colored aluminum alloy product are provided to obtain predetermined color comparing with aluminum before coloring or a material made of aluminum alloy and to improve thermal resistance.;CONSTITUTION: A method for manufacturing colored aluminum product or colored aluminum alloy product comprises: a step of processing a material made of aluminum or aluminum alloy with anodic oxidation process among process solution containing phosphoric acid and forming an anodic oxidation film including a plurality of air holes on a surface of the material; a step of processing the material with hot water at 40-100 deg. C; and a step of dipping the material among color composition for coloring containing color particle, dispersing agent, and water and coloring by filling the color particle into the air holes existing to the anodic oxidation film.;COPYRIGHT KIPO 2013
机译:目的:提供一种在不降低色度或着色铝合金产品的情况下制造着色铝产品的方法,用于着色的颜色组合物和着色铝产品或着色铝合金产品,以获得与着色前的铝或由铝制成的材料相比预定的颜色组成:一种有色铝产品或有色铝合金产品的制造方法,包括:在含磷酸的工艺溶液中,通过阳极氧化工艺处理铝或铝合金制成的材料并形成阳极的步骤。该氧化膜在该材料的表面上包括多个气孔。用40-100度的热水处理材料的步骤。 C;通过将着色颗粒填充到存在于阳极氧化膜中的气孔中,将包含着色颗粒,分散剂和水的着色材料浸入着色用着色组合物中的步骤。; COPYRIGHT KIPO 2013

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号