PROBLEM TO BE SOLVED: To provide a conductive oxide fine particle dispersion liquid for forming a transparent conductive film for a super straight type solar cell and the transparent conductive film formed using the dispersion liquid, which greatly reduce contact resistance in a longitudinal direction with respect to the film and, as a result, when constituting a solar cell, increase a fill factor which is one of the factors that determine conversion efficiency, as well as a composite film and a method of manufacturing them.;SOLUTION: The conductive oxide fine particle dispersion liquid used to manufacture a transparent conductive film formed on a photoelectric conversion layer of the super straight type solar cell and constituted by a first layer containing a binder component and a second layer formed on the first layer and containing a less binder component compared with the first layer is prepared by dispersing the conductive oxide fine particles in a dispersion medium, and it is adjusted so that, assuming that a frequency of all particles of the conductive oxide fine particles in a number-based particle size distribution is 100%, the frequency of particles whose diameters are 50 nm or more is 70-100% and also the frequency of particles whose diameters are 200 nm or more is 10% or less.;COPYRIGHT: (C)2011,JPO&INPIT
机译:解决的问题:提供用于形成用于超直型太阳能电池的透明导电膜的导电氧化物细粒分散液和使用该分散液形成的透明导电膜,其大大减小了相对于纵向的接触电阻。薄膜,结果,当构成太阳能电池时,增加了决定转换效率的因素之一的填充系数,以及复合薄膜及其制造方法。用于制造透明导电膜的分散液,该透明导电膜形成在超直型太阳能电池的光电转换层上,并且由包含粘合剂组分的第一层和形成在第一层上且与粘合剂层相比包含较少的粘合剂组分的第二层构成通过将导电氧化物微粒分散在分散介质中来制备第一层,假设在基于数量的粒径分布中,导电氧化物细颗粒的所有颗粒的频率为100%,则直径为50 nm或更大的颗粒的频率为70-100%,并且直径大于等于200 nm的颗粒等于或小于10%。;版权所有:(C)2011,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号