the subject of the invention is a new way to produce composite cellulose and zinc oxide (ii) using ionic liquids cykloheksyloamoniowych applicable as fillers in the production of plastics.in a variety of way new composite cellulose and zinc oxide (ii) using cykloheksyloamoniowych ionic liquids is that liquid ionic specified general model 1 in which r is an alkyl substituent prostou0142au0144cuchowy composed of 1 to 20 carbon atoms, l or benzyl or allyl substituent.and and the rest of the acidic organic acids added cellulose in temperature from 20 to 120u00b0c, in quantities of from 0.05 to 30% by weight, then after reconstitution following zinc oxide (ii) in quantities of from 0.01 to 50% by weight calculated on the amount of added previously cellulose, followed by boiled solution cools and added to the solvent.the crystallized cellulose composite material and zinc oxide (ii) odsu0105cza and drought in temperature from 20 to 60u00b0c, for a period of 1 do48 hours.
机译:发明内容本发明的主题是使用离子液体cykloheksyloamoniowych制备复合纤维素和氧化锌(ii)的新方法,其可用作塑料生产中的填充剂。以多种方式使用cykloheksyloamoniowych离子液体新的复合纤维素和氧化锌(ii)是液体离子指定的通用模型1,其中r是由1至20个碳原子,l或苄基或烯丙基取代基组成的烷基取代基,而其余酸性有机酸在20至20到120 u00b0c,以0.05至30重量%的量添加到120 u00b0c中,然后在复溶后,以预先添加的纤维素量为基准,以0.01至50重量%的氧化锌(ii)进行冷却,然后煮沸的溶液冷却并将结晶的纤维素复合材料和氧化锌(ii)ods溶解并在20至60的温度下干旱1至48小时。

著录项

  • 公开/公告号PL400207A1

    专利类型

  • 公开/公告日2014-02-03

    原文格式PDF

  • 申请/专利权人 POLITECHNIKA POZNAŃSKA;

    申请/专利号PL20120400207

  • 发明设计人 JULIUSZ PERNAK;ROKSANA KORDALA;

    申请日2012-08-01

  • 分类号C08J3/11;C08L1/02;C08K3/22;

  • 国家 PL

  • 入库时间 2022-08-21 15:56:31

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号