ENERGY-SAVING AND ENVIRONMENT PROTECTIVE METHOD FOR PREPARING GLASS WITH HIGH INTENSITY

机译:一种高强度玻璃的节能环保方法

摘要

A glass preparation process and its glass product, comprising the following steps: step 1: the raw materials are prepared for glass manufacturing according to the compositions contained in the said glass such as SiO2, CaO, MgO, Al2O3, Fe2O3 and Na2O; step 2: after the prepared raw materials are measured, they are put into the bulk material pipe or feed bin; step 3: put the formulated raw materials into molten pool to have them melted under the melting temperature of each glass formula and form the liquid glass with preset viscosity, then they are homogenized and clarified and discharge bubbles to form flowing molten mass; step 4: tube-drawing molding process, blowing molding process or compression molding process is selected and adopted for molding.
机译:一种玻璃的制备方法及其玻璃产品,包括以下步骤:步骤1:根据所述玻璃中所含的组成如SiO 2 ,CaO,MgO, Al 2 O 3 ,Fe 2 O 3 和Na 2 O;步骤2:对准备好的原料进行计量后,将其放入散料管或进料箱中。步骤3:将配制好的原料放入熔池中,使其在每种玻璃配方的熔融温度下熔融,形成具有预定粘度的液态玻璃,然后进行均质澄清,排出气泡,形成流动的熔体。步骤4:选择拉管成型工艺,吹塑成型工艺或压缩成型工艺进行成型。

著录项

  • 公开/公告号US2015299027A1

    专利类型

  • 公开/公告日2015-10-22

    原文格式PDF

  • 申请/专利权人 DENING YANG;

    申请/专利号US201113985411

  • 发明设计人 DENING YANG;

    申请日2011-03-15

  • 分类号C03C3/091;C03B19/02;C03C3/064;C03B27/012;C03C3/087;C03C3/062;C03B9/30;C03B17/04;

  • 国家 US

  • 入库时间 2022-08-21 15:27:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号