首页> 外国专利> METHOD FOR PRODUCING CONCAVE-CONVEX SUBSTRATE USING SOL-GEL METHOD, SOL SOLUTION USED IN SAME, METHOD FOR PRODUCING ORGANIC EL ELEMENT USING SAME, AND ORGANIC EL ELEMENT OBTAINED THEREBY

METHOD FOR PRODUCING CONCAVE-CONVEX SUBSTRATE USING SOL-GEL METHOD, SOL SOLUTION USED IN SAME, METHOD FOR PRODUCING ORGANIC EL ELEMENT USING SAME, AND ORGANIC EL ELEMENT OBTAINED THEREBY

机译:使用溶胶-凝胶法制造凹形凸物的方法,在同一溶液中使用的固溶体,通过使用相同方法制造有机元素的方法以及由此获得的有机元素

摘要

A method for producing a substrate having a concavity and convexity pattern includes: a step S2 for applying a sol containing a silica precursor on a substrate to form a coating film; a step S3 for drying the coating film; a pressing step S4 for pressing a mold having a concavity and convexity pattern against the dried coating film with a pressing roll; a step S6 for peeling off the mold from the coating film; and a step S7 for baking the coating film to which the concavity and convexity pattern has been transferred. The coating film is dried in the drying step so that the ratio of weight of the coating film to dried weight of the coating film is in a range of 1.4 to 8.8, the dried weight being obtained by baking the coating film at a temperature of 100 degrees Celsius. The coating film may be heated in the pressing step.
机译:用于制造具有凹凸图案的基板的方法包括:步骤S2,用于将包含二氧化硅前体的溶胶涂布在基板上以形成涂膜;步骤S3,使涂膜干燥。压制步骤S4,其利用压辊将具有凹凸图案的模具压在干燥后的涂膜上。步骤S6,从涂膜上剥离模具。步骤S7,用于烘烤已转印有凹凸图案的涂膜。在干燥步骤中干燥涂膜,使得涂膜的重量与涂膜的干燥的重量之比在1.4至8.8的范围内,干燥的重量通过在100℃的温度下烘烤涂膜而获得。摄氏度。可以在加压步骤中加热涂膜。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号