摘要

FIELD: electricity.;SUBSTANCE: method of fabrication of nickel oxide electrode for nickel-zinc battery includes impregnation of the ready electrode in the solution containing in g/l: cobalt sulphate 50-75, cadmium sulphate 50-75 g/l, within 0.5-1.0 hours, the subsequent processing in potassium alkali solution with the concentration 200-300 g/l within 0.5-1.0 hours and final formation of the electrode in the potassium alkali solution with the concentration 1-3 mol/l at the charging and discharging density of the current 2-10 mA/cm2.;EFFECT: increase of capacity of nickel-zinc batteries with nickel oxide and zinc electrodes at the short discharge modes.;1 dwg, 1 ex
机译:领域:电力;物质:用于镍锌电池的氧化镍电极的制造方法包括将就绪电极浸入以下溶液中:g / l:硫酸钴50-75,硫酸镉50-75 g / l 0.5-1.0小时,随后在0.5-1.0小时内在浓度为200-300 g / l的碱金属钾溶液中进行处理,并最终在充电时在浓度为1-3 mol / l的碱金属钾溶液中形成电极。电流2-10 mA / cm 2 的放电密度。效果:在短放电模式下,带有氧化镍和锌电极的镍锌电池容量增加。1dwg,1 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号