An improved process for the preparation of phosphorous containing mesoporous alumina calalyst for selective dehydration of methanol to dimethyl ether

机译:一种制备含磷介孔氧化铝催化剂的改进方法,该催化剂用于将甲醇选择性脱水成二甲醚

摘要

The present invention provide an improved process for the preparation of phosphorous containing mesoporous alumina catalyst for selective dehydration of methanol to dimethyl ether. The process provides a single step selective vapour phase dehydration of methanol to produce dimethyl ether over phosphorous containing mesoporous alumina (P/Al203) catalyst at a temperature 250 -300°C. The process provides methanol conversion of 45-1 00% with selectivity up to 100%.
机译:本发明提供了一种制备含磷的介孔氧化铝催化剂的改进方法,该催化剂用于将甲醇选择性脱水成二甲醚。该方法提供了甲醇的一步选择性汽相脱水,以在含磷的中孔氧化铝(P / Al 2 O 3)催化剂上在250 -300℃的温度下生产二甲醚。该方法提供了45-1 00%的甲醇转化率,选择性高达100%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号