首页> 外国专利> ALUMINIUM ALLOY FOR PRODUCING SEMI FINISHED PRODUCTS OR COMPONENTS FOR MOTOR VEHICLES METHOD FOR PRODUCING AN ALUMINIUM ALLOY STRIP CONSISTING OF THIS ALUMINIUM ALLOY AND AN ALUMINIUM ALLOY STRIP AND USE FOR SAME

ALUMINIUM ALLOY FOR PRODUCING SEMI FINISHED PRODUCTS OR COMPONENTS FOR MOTOR VEHICLES METHOD FOR PRODUCING AN ALUMINIUM ALLOY STRIP CONSISTING OF THIS ALUMINIUM ALLOY AND AN ALUMINIUM ALLOY STRIP AND USE FOR SAME

机译:用于生产半成品或汽车零部件的铝合金生产铝合金条的方法构成这种铝合金和铝合金条的方法及其用途

摘要

The invention relates to an aluminium alloy for producing semi finished products or components for motor vehicles in which the alloy constituents of the aluminium alloy have the following proportions in wt.%: Fe = 0.80 % Si = 0.50 % 0.90 % = Mn = 1.50 % Mg = 0.25 % Cu = 0.125 % Cr = 0.05 % Ti = 0.05 % V = 0.05 % Zr = 0.05 % the remainder being aluminium and inevitable accompanying elements at 0.05 % individually and 0.15 % in total and the combined proportion of Mg and Cu satisfying the following relation in wt.%: 0.15 % = Mg + Cu = 0.25 % where the proportion of Mg in the aluminium alloy is greater than the proportion of Cu in the aluminium alloy. The invention also relates to a method for producing an aluminium alloy strip from such an aluminium alloy comprising the following steps: casting a rolling ingot consisting of a claimed aluminium alloy homogenising the rolling ingot at 480�C to 600�C for at least 0.5 h hot rolling the rolling ingot at 280�C to 500�C to form an aluminium alloy strip cold rolling the aluminium alloy strip to its final thickness followed by the re crystallising final annealing of said aluminium alloy strip. The invention also relates to an aluminium alloy strip produced according to this method as well as to uses for the claimed aluminium alloy and a metal sheet produced from the claimed aluminium alloy strip.
机译:本发明涉及一种用于生产汽车半成品或部件的铝合金,其中铝合金的合金成分具有以下重量百分比:Fe = 0.80%Si = 0.50%0.90%= Mn = 1.50% Mg = 0.25%Cu = 0.125%Cr = 0.05%Ti = 0.05%V = 0.05%Zr = 0.05%其余为铝和不可避免的伴随元素,其含量分别<0.05%和总量<0.15%,并且Mg和以重量%满足以下关系的Cu:0.15%= Mg + Cu = 0.25%,其中铝合金中Mg的比例大于铝合金中Cu的比例。本发明还涉及一种由这种铝合金生产铝合金带的方法,该方法包括以下步骤:铸造由要求保护的铝合金组成的轧制锭,将轧制锭在480℃至600℃下均化至少0.5h。将轧制锭料在280°C至500°C的温度下热轧以形成铝合金带材,将铝合金带材冷轧至最终厚度,然后对该铝合金带材进行再结晶最终退火。本发明还涉及根据该方法生产的铝合金带以及用于要求保护的铝合金的用途和由要求保护的铝合金带制造的金属板。

著录项

  • 公开/公告号IN2015KN02436A

    专利类型

  • 公开/公告日2016-06-24

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN2436/KOLNP/2015

  • 申请日2015-07-27

  • 分类号C22C21/00;C22F1/04;B62D29/00;

  • 国家 IN

  • 入库时间 2022-08-21 14:24:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号