The method for producing MTW type zeolite of the present invention comprises mixing a silica source, an alumina source, an alkali source, a lithium source, and water so as to be a reaction mixture having a composition represented by a specific molar ratio,2/ Al2O3MTW type zeolite containing no organic compound having a ratio of 10 to 500 is used as a seed crystal and added to the reaction mixture in a proportion of 0.1 to 20% by weight based on the silica component in the reaction mixture. (3) And the reaction mixture to which the crystals have been added is sealed and heated at 100 to 200 C.
展开▼
机译:本发明的MTW型沸石的制造方法包括将二氧化硅源,氧化铝源,碱源,锂源和水混合,以成为具有由特定摩尔比表示的组成的反应混合物。不包含比例为10到500的有机化合物的> 2 Sub> / Al 2 Sub> O 3 Sub> MTW型沸石用作晶种并添加到反应中相对于反应混合物中的二氧化硅组分,混合物的比例为0.1-20重量%。 (3)然后,将添加了晶体的反应混合物密封,并在100〜200℃下加热。