PROBLEM TO BE SOLVED: To provide a glass plate with a low-reflection coating that can exert high photocatalytic activity.SOLUTION: The glass plate with a low-reflection coating comprises: a glass plate; and a low-reflection coating which includes binder having silica as a main component, silica microparticles fixed by the binder, and titania microparticles fixed by the binder and is formed at least on a part of one main surface of the glass plate. The low-reflection coating satisfies a relationship C25 mass% when 30 mass%C68 mass%, 12 mass%≤C50 mass%, 20 mass%C43.75 mass%, C/C≥0.6, C≥55 mass%, and satisfies a relationship C20 mass% when C55 mass%. The glass plate with a low-reflection coating has a transmittance gain of 2.0% or more.SELECTED DRAWING: None
机译:解决的问题:提供一种具有低反射涂层的玻璃板,该玻璃板可以发挥高的光催化活性。解决方案:该具有低反射涂层的玻璃板包括:至少在玻璃板的一个主表面的一部分上形成有低反射涂层,该低反射涂层包括以二氧化硅为主要成分的粘合剂,由该粘合剂固定的二氧化硅微粒和由该粘合剂固定的二氧化钛微粒。当30质量%<C <68质量%,12质量%≤C<50质量%,20质量%<C <43.75质量%,C /C≥0.6时,低反射膜满足C <25质量%的关系。 C≥55质量%,当C <55质量%时满足关系C> 20质量%。带有低反射涂层的玻璃板的透射率增益为2.0%或更高。

著录项

  • 公开/公告号JP2018017888A

    专利类型

  • 公开/公告日2018-02-01

    原文格式PDF

  • 申请/专利权人 NIPPON SHEET GLASS CO LTD;

    申请/专利号JP20160148026

  • 申请日2016-07-28

  • 分类号G02B1/111;B05D7/24;B05D3;B05D3/02;B05D5/06;C03C17/25;C09D5;C09D7/40;C09D201;C09D183;

  • 国家 JP

  • 入库时间 2022-08-21 13:11:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号