One embodiment of the present invention provides a green cement composition comprising Portland cement, carbon minerals, an early strength type expansion agent, and blast furnace slag micropowder. In one embodiment of the present invention: carbon minerals obtained by reacting carbon dioxide, which is a main cause of greenhouse gas, with cogeneration plant fly ash are used, and thus the green cement composition has an effect of better reducing the amount of carbon dioxide than a conventional green cement, which has a simple mixture of fly ash and blast furnace slag micropowder; the cogeneration plant fly ash, which was restricted when used as a concrete admixture because of a high content of free lime, can be effectively utilized; and early strength deterioration and drying shrinkage, which are problems of the conventional green cement, are reduced using the early strength type expansion agent.
机译:本发明的一个实施方案提供了一种生水泥组合物,其包含波特兰水泥,碳矿物质,早期强度型膨胀剂和高炉矿渣微粉。在本发明的一个实施方案中:使用了通过使作为温室气体的主要原因的二氧化碳与热电联产植物粉煤灰反应获得的碳矿物质,因此绿色水泥组合物具有更好地减少二氧化碳量的效果。与传统的绿色水泥相比,传统的绿色水泥具有粉煤灰和高炉矿渣微粉的简单混合物;可有效利用热电联产植物粉煤灰,该粉煤灰由于游离石灰含量高而在用作混凝土掺合料时受到限制。使用早期强度型膨胀剂可以减少常规生水泥的问题,即早期强度劣化和干燥收缩。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号