Aluminum alloy products, such as plate, forgings and extrusions, suitable for use in making aerospace structural components like integral wing spars, ribs and webs, comprises about: 6 to 10 wt. % Zn; 1.2 to 1.9 wt. % Mg; 1.2 to 2.2 wt. % Cu, with Mg≤(Cu+0.3); and 0.05 to 0.4 wt. % Zr, the balance Al, incidental elements and impurities. Preferably, the alloy contains about 6.9 to 8.5 wt. % Zn; 1.2 to 1.7 wt. % Mg; 1.3 to 2 wt. % Cu. This alloy provides improved combinations of strength and fracture toughness in thick gauges. When artificially aged per the 3-stage method of preferred embodiments, this alloy also achieves superior SCC performance, including under seacoast conditions.
机译:适用于制造航空结构部件(如整体翼梁,肋和腹板)的铝合金产品(例如板,锻件和挤压件)约占重量的6%至10%。锌; 1.2至1.9 wt。镁含量1.2至2.2 wt。 %Cu,含Mg≤(Cu + 0.3);和0.05至0.4重量%。 %Zr,余量的Al,附带的元素和杂质。优选地,合金包含约6.9至8.5重量%。锌; 1.2至1.7 wt。镁含量1.3至2 wt。铜含量这种合金在厚规格中提供了强度和断裂韧性的改进组合。当按照优选实施方案的3阶段方法进行人工时效时,该合金还实现了优异的SCC性能,包括在海岸条件下。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号