[Task] Performance improvement and cost reduction in a positive electrode active material for a lithium ion battery. [Means for Resolution] A method of manufacturing a lithium nickel composite oxide including the following Steps 1 to 7: (Step 1) a dissolving step; (Step 2) a precipitation step; (Step 3) a filtering step; (Step 4) a drying step; (Step 5) a mixing step of mixing aluminum hydroxide and lithium carbonate with the precursor powder, which is obtained in Step 4, to obtain a mixture; (Step 6) a high-temperature firing step of firing the mixture, which is obtained in Step 5, at a high temperature of higher than 790°C to obtain a fired product; and (Step 7) a low-temperature firing step of firing the fired product, which has undergone Step 6, at a low temperature of lower than 790°C.
机译:[任务]锂离子电池用正极活性物质的性能提高和成本降低。 [解决方案]一种锂镍复合氧化物的制造方法,包括以下步骤1至7:(步骤1)溶解步骤;和(步骤2)沉淀步骤; (步骤3)过滤步骤; (步骤4)干燥步骤; (步骤5)混合步骤,将氢氧化铝和碳酸锂与在步骤4中获得的前体粉末混合,以获得混合物; (步骤6)高温烧制步骤,将步骤5中获得的混合物在高于790℃的高温下烧制以获得烧制产物; (步骤7)在低于790℃的低温下对经过了步骤6的烧成物进行烧成的低温烧成步骤。

著录项

  • 公开/公告号PL3228595T3

    专利类型

  • 公开/公告日2019-09-30

    原文格式PDF

  • 申请/专利权人 UMICORE;

    申请/专利号PL20150865101T

  • 申请日2015-12-01

  • 分类号C01G53;H01M4/02;H01M4/505;H01M4/525;H01M10/0525;

  • 国家 PL

  • 入库时间 2022-08-21 12:01:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号