CHROMIUM-NICKEL-BASED ALLOY FOR RADIANT TUBE, HAVING EXCELLENT HIGH-TEMPERATURE DEFORMATION RESISTANCE AND CRACK RESISTANCE, AND MANUFACTURING METHOD THEREFOR
CHROMIUM-NICKEL-BASED ALLOY FOR RADIANT TUBE, HAVING EXCELLENT HIGH-TEMPERATURE DEFORMATION RESISTANCE AND CRACK RESISTANCE, AND MANUFACTURING METHOD THEREFOR
展开▼
机译:具有出色的高温抗变形和抗裂性能的铬镍基耐高温管合金及其制造方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
The present invention relates to a Cr-Ni-based alloy for a radiant tube, having excellent resistance to high-temperature deformation and cracks, and a manufacturing method therefor. One embodiment of the present invention provides: a Cr-Ni-based alloy for a radiant tube, having excellent high-temperature deformation resistance and crack resistance, the Cr-Ni-based alloy comprising, by wt%, 0.17-0.3% of carbon (C), 30-35% of chromium (Cr), 45-55% of nickel (Ni), 1% or less of manganese (Mn), 1% or less of silicon (Si), 1-3% of one of niobium (Nb) and vanadium (V) or the sum of the both, 5-18% of tungsten (W), 0.1-1.5% of tantalum (Ta), 0.1-1.5% of hafnium (Hf), 0.001-0.02% of boron (B), 0.05-1.5% of yttrium (Y) and the balance of Fe and other inevitable impurities, and having an average interval between solidified dendrites of 30 μm or less; and a manufacturing method therefor.
展开▼