A fiber-reinforced thermoplastic resin prepreg that is a fiber-reinforced polyamide prepreg which contains (A) reinforcing fibers, (B) a sizing agent and (C) a polyamide resin, and wherein the sizing agent (B) and the polyamide resin (C) satisfy the following condition. N m /N 0 4.0 (No is the average of torques necessary for maintaining the number of revolutions of a roller type blade at 100 rpm/15 minutes, said average representing the fluidity of the polyamide resin (C) in cases where only the polyamide resin (C) is filled into a mixer having the roller type blade and heated and melted at a temperature that is higher than the melting point of the polyamide resin (C) by 30°C; and N m is the average of torques necessary for maintaining the number of revolutions of a roller type blade at 100 rpm/15 minutes, said average representing the fluidity of a mixture, which is obtained by mixing the sizing agent (B) and the polyamide resin (C) at 3:100 (mass ratio), in cases where the mixture is filled into a mixer having the roller type blade and heated and melted at a temperature that is higher than the melting point of the polyamide resin (C) by 30°C.)
机译:纤维增强热塑性树脂预浸料,其为纤维增强聚酰胺预浸料,其包含(A)增强纤维,(B)上浆剂和(C)聚酰胺树脂,并且其中所述上浆剂(B)和所述聚酰胺树脂( C)满足以下条件。 N m / N 0 <4.0(No是将辊式刀片的转数保持在100 rpm / 15分钟所需的平均扭矩,该平均值代表仅在树脂基体中聚酰胺树脂(C)的流动性将聚酰胺树脂(C)填充到具有辊式叶片的混合器中,并在比聚酰胺树脂(C)的熔点高30℃的温度下加热并熔融;并且N m是所需扭矩的平均值。为了将辊式刀片的转数保持在100 rpm / 15分钟,所述平均值代表混合物的流动性,该混合物是通过将上浆剂(B)和聚酰胺树脂(C)以3:100的比例混合而获得的( (质量比),将混合物填充到具有辊型叶片的混合器中,并在比聚酰胺树脂(C)的熔点高30℃的温度下加热并熔融的情况下)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号