首页> 外国专利> Glaze composition for chemical strengthening of bone china earthenware and manufacturing method of bone china earthenware using the glaze composition

Glaze composition for chemical strengthening of bone china earthenware and manufacturing method of bone china earthenware using the glaze composition

机译:用于化学强化骨瓷陶器的釉料组合物和使用该釉料组合物的骨瓷陶器的制造方法

摘要

The present invention relates to a chemical strengthening glaze composition for bone china ceramics and a producing method of bone china ceramics using the same. The chemical composition of the glaze composition, which is enameled on the surface of bone china ceramics and is treated with chemical strengthening to form a chemical strengthening glaze layer, includes 55-63 wt% of SiO_2, 10-14 wt% of Al_2O_3, 1-6 wt% of B_2O_3, 0.1-5 wt% of CaO, 1-6 wt% of MgO, 0.5-4 wt% of K_2O, 10-15 wt% of Na_2O, 0.1-4 wt% of Li_2O, and 1-8 wt% of ZnO as a chemical composition. The present invention is able to suppress the occurrence of fine cracks or scratches on the surface of bone china ceramics and improve mechanical properties such as strength and hardness.
机译:本发明涉及用于骨瓷陶瓷的化学增强釉组合物和使用该组合物的骨瓷陶瓷的生产方法。釉料组合物的化学成分被涂在骨瓷陶瓷的表面并经过化学强化处理以形成化学强化釉层,该化学成分包括55-63 wt%的SiO_2、10-14 wt%的Al_2O_3、1 -6 wt%的B_2O_3、0.1-5 wt%的CaO,1-6 wt%的MgO,0.5-4 wt%的K_2O,10-15 wt%的Na_2O,0.1-4 wt%的Li_2O和1- 8 wt%的ZnO作为化学成分。本发明能够抑制在骨瓷陶瓷表面上出现细裂纹或划痕,并改善机械性能,例如强度和硬度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号