The removal of metal impurities from metallurgical grade silicon (MG-Si) by acid leaching has been investigated with the addition of CaO. Prior to adding CaO, Fe is the main impurity in the MG-Si sample, and the 2nd-phase precipitates in silicon are Si-Fe-based alloys, such as Si-Fe, Si-Fe-Ti, Si-Fe-Al, Si-Fe-Mn, and Si-Fe-Ni. The phases of Si-Fe and Si-Fe-Ti are not appreciably soluble in HCl. After the introduction of CaO, Ca becomes the dominant impurity, and the 2nd-phase precipitates become Si-Fe-based alloys, such as Si-Ca, Si-Ca-(Fe, Ti, Ni, Al), and Si-Ca-Fe-Al. These are effectively leached with HCl. Therefore, the HCl leaching effect on the removal of metal impurities has been improved. The optimum content of Ca in the MG-Si samples after adding CaO is in the range of 1 pct to 4 pct, the contents of Fe, Al, Ti, and Ni have been decreased to a minimum of less than 5 ppmw (ppm by weight) each, and the acid leaching results do not show a dependence on Ca content at this range.
机译:已经研究了通过添加CaO来通过酸浸从冶金级硅(MG-Si)中去除金属杂质的方法。在添加CaO之前,Fe是MG-Si样品中的主要杂质,硅中的第二相沉淀是Si-Fe基合金,例如Si-Fe,Si-Fe-Ti,Si-Fe-Al ,Si-Fe-Mn和Si-Fe-Ni。 Si-Fe和Si-Fe-Ti相明显不溶于HCl。引入CaO后,Ca成为主要杂质,第二相沉淀物变为Si-Fe基合金,例如Si-Ca,Si-Ca-(Fe,Ti,Ni,Al)和Si-Ca -铁铝这些用HCl有效地浸出。因此,提高了HCl对金属杂质去除的浸出效果。添加CaO后,MG-Si样品中的Ca的最佳含量在1%至4%的范围内,Fe,Al,Ti和Ni的含量已降低至最小小于5 ppmw(ppm酸浸出的结果在该范围内不依赖于Ca含量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号