Evaluation of bond strength of different adhesive systems: Shear and Microtensile Bond Strength Test

机译:评估不同粘合剂体系的粘合强度:剪切和微拉伸粘合强度试验

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Aim of this work is the in vitro bond strength evaluation of three bonding agents comparing the results of two kinds of test, Microtensile Bond Strength Test and a Shear Bond Strength Test. Bond strength tests have been used to test both direct and indirect restorative techniques to investigate if methods could give different results.ud72 human third molars have been collected and stored in physiological solution. Three kinds of test were conducted: 1- SB, 2- “Slice” preparation μTBS1, 3- “Stick” preparation μTBS2. We tested three different adhesive systems (Groups 1-2-3 n=24), two restorative techniques (subgroup A–B n=12). The tested adhesives were: Optibond FL (OFL) (Group 1), Optibond Solo Plus (OSP) (Group 2), Optibond Solo Plus Self-Etch (OSSE) (Group 3). For all tests was used a universal load machine Instron Machine.udBest values were found for Optibond FL with mean values of 45–50 MPa. Optibond Solo Plus resulted in values very similar and in some cases almost identical to FL. Optibond Solo Self Etch showed poorer adhesion in both direct and indirect restorative techniques. The parametric and non parametric statistical variance analysis pointed out the absence of significant differences between OFL and OSP, and demonstrated a significant difference for OSSE adhesive.udThe results confirm that a total etch two-step adhesive is the best compromise between easiness and effectiveness.ud
机译:这项工作的目的是对三种粘合剂的体外粘合强度进行评估,比较两种测试的结果:微拉伸粘合强度测试和剪切粘合强度测试。粘结强度测试已用于测试直接和间接修复技术,以研究方法是否可以得出不同的结果。 ud72人的第三磨牙已被收集并存储在生理溶液中。进行了三种测试:1-SB,2-“切片”制备μTBS1,3-“ Stick”制备μTBS2。我们测试了三种不同的粘合剂系统(1-2-3组,n = 24),两种修复技术(A-B组,n = 12)。测试的粘合剂为:Optibond FL(OFL)(第1组),Optibond Solo Plus(OSP)(第2组),Optibond Solo Plus自蚀刻(OSSE)(第3组)。对于所有测试,均使用万能负载机Instron Machine。 ud发现Optibond FL的最佳值为45–50 MPa的平均值。 Optibond Solo Plus产生的值非常相似,在某些情况下几乎与FL相同。 Optibond Solo Self Etch在直接和间接修复技术中均显示较差的附着力。参数和非参数统计方差分析指出,OFL和OSP之间不存在显着差异,并证明OSSE粘合剂具有显着差异。 ud结果证实,全蚀刻两步粘合剂是易用性和有效性之间的最佳折衷方案。 ud