High-Pressure Micellar Solutions of Polystyrene-block-polybutadiene and Polystyrene-block-polyisoprene in Propane Exhibit Cloud-Pressure Reduction and Distinct Micellization End Points

机译:聚丙烯 - 嵌段 - 聚丁二烯和聚苯乙烯 - 嵌段 - 聚异戊二烯在丙烷中的高压胶束溶液表现出云压降低和不同的胶束化终点

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Micellar solutions of polystyrene-block-polybutadiene and polystyrene-block-polyisoprene in propane are found to exhibit significantly lower cloud pressures than the corresponding hypothetical nonmicellar solutions. Such a cloud-pressure reduction indicates the extent to which micelle formation enhances the apparent diblock solubility in near-critical and hence compressible propane. Concentration-dependent pressure-temperature points beyond which no micelles can be formed, referred to as the micellization end points, are found to depend on the block type, size, and ratio. The cloud-pressure reduction and the micellization end point measured for styrene-diene diblocks in propane should be characteristic of all amphiphilic diblock copolymer solutions that form micelles in compressible solvents.
机译:发现丙烷中的聚苯乙烯嵌段聚丁二烯和聚苯乙烯嵌段聚异戊二烯的胶束溶液比相应的假设非胶束溶液显示出明显更低的云压。这种云压降低表明胶束形成增强了在近临界且因此可压缩的丙烷中的表观二嵌段溶解度的程度。发现取决于浓度的压力-温度点,超过该温度-点不能形成胶束,称为胶束化终点,这取决于嵌段的类型,大小和比例。丙烷中苯乙烯-二烯二嵌段测得的云压降低和胶束化终点应是所有在可压缩溶剂中形成胶束的两亲性二嵌段共聚物溶液的特征。