Anatase TiO2 was prepared by sol-gel method through the hydrolysis of TiCl4. Ni2+ was doped into the TiO2 matrix in the concentration range of 0.02 to 0.1 at. and characterized by various analytical techniques. Powder X-ray diffraction revealed only anatase phase for all the samples, while diffuse reflectance spectral studies indicated a red shift in the band gap absorption to the visible region. The photocatalytic activities of these photocatalysts were probed for the degradation of methyl orange under natural solar light. The photocatalyst with optimum doping of 0.08 at. Ni2+, showed enhanced activity, which is attributed to: (i) effective separation of charge carriers and (ii) large red shift in the band gap to visible region. The influence of crystallite size and dopant concentration on the charge carrier trapping - recombination dynamics is investigated. © Versita Warsaw and Springer-Verlag Berlin Heidelberg.
机译:锐钛矿型TiO2是通过溶胶-凝胶法通过TiCl4的水解制备的。将Ni 2+以0.02至0.1at。%的浓度范围掺杂到TiO 2基体中。并具有各种分析技术的特点。粉末X射线衍射显示所有样品仅具有锐钛矿相,而漫反射光谱研究表明带隙吸收向可见区有红移。探究了这些光催化剂的光催化活性,以了解在自然太阳光下甲基橙的降解情况。最佳掺杂量为0.08 at。的光催化剂。 Ni 2+表现出增强的活性,这归因于:(i)电荷载流子的有效分离和(ii)带隙至可见区的大红移。研究了微晶尺寸和掺杂剂浓度对电荷载流子俘获-复合动力学的影响。 ©Versita华沙和Springer-Verlag柏林海德堡。