首页> 外文OA文献 >Application of design of experiment techniques in the two step pretreatment proses for diamond coating
【2h】

Application of design of experiment techniques in the two step pretreatment proses for diamond coating

机译:实验技术设计在金刚石涂层两步预处理中的应用

摘要

Chemical vapor Deposition (CVD) is one of diamond synthesis process and it is widely applied to cutting tools to enhance wear resistance and increase tool life. One of the methods of ensuring adhesion of diamond on the substrate is through the roughening and the substrate surface and the removal of cobalt at the substrate surface. This method is applied during the pretreatment method, which is before the coating process. In this study, Murakami etchant was used to roughen the surface and this is followed by an acid treatment to remove cobalt at the Tungsten Carbide (WC- 6% Co) surface. Concentration of both solutions has been varied. Design of Experiment Techniques has been used to determine the optimum combination of the factor that has been investigated. Result from this study shows the optimum condition for maximizing the surface roughness is 10.23g of potassium ferricyanide, 29.92g of potassium hydroxide and etching time in ultrasonic bath of 19.74 minutes while the optimum concentration for acid treatment is 60.36% for nitric acid, 10.29% of hydrogen peroxide and 89.43 seconds for etching time.
机译:化学气相沉积(CVD)是金刚石合成工艺之一,它广泛应用于切削工具以增强耐磨性并延长工具寿命。确保金刚石在基底上粘附的方法之一是通过粗糙化和基底表面以及除去基底表面的钴。在涂覆方法之前的预处理方法中应用此方法。在这项研究中,村上蚀刻剂用于使表面变粗糙,然后进行酸处理以去除碳化钨(WC-6%Co)表面的钴。两种溶液的浓度都不同。实验技术的设计已用于确定已研究因素的最佳组合。研究结果表明,使表面粗糙度最大的最佳条件是铁氰化钾10.23g,氢氧化钾29.92g,超声浴中蚀刻时间为19.74分钟,而硝酸的最佳酸处理浓度为60.36%,硝酸为10.29%。的过氧化氢和89.43秒的蚀刻时间。

著录项

  • 作者

    Husin Norafifah;

  • 作者单位
  • 年度 2009
  • 总页数
  • 原文格式 PDF
  • 正文语种 {"code":"en","name":"English","id":9}
  • 中图分类

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号