Extraction and characterization of cellulosic nanowhisker obtained from discarded cotton fibers

机译:废弃棉纤维中纤维素纳米晶须的提取与表征

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

This study aimed to characterize cellulose nanowhiskers extracted from discarded cotton fibers. The nanocellulose was characterized by dynamic light scattering, zeta potential, Scanning Transmission Electron Microscopy (STEM), Atomic force microscopy (AFM) and X-ray powder diffraction (XRD). The nanocrystals are characterized by a rod-like morphology with sizes between 100 nm and 300 nm. The acidic hydrolyses applied to the extract nanocrystals increased the crystallinity index from 72 to 86%. The average length and diameter obtained were 98.1±4.7 and 8.0±3.4 nm, respectively. The aspect ratio of the fibers, around 12.3, was lower than the values usually reported in the literature. The dynamic light scattering results were in accordance with the nano crystal dimensions showing an average size of 235 nm. Cellulose nanowhiskers obtained from cotton rejected by textile industry due to their abundance, low cost, high crystallinity, strength, low weight and biodegradability, are the ideal candidates for the processing of polymer nanocomposites.
机译:这项研究旨在表征从废弃棉纤维中提取的纤维素纳米晶须。纳米纤维素的特征在于动态光散射,ζ电势,扫描透射电子显微镜(STEM),原子力显微镜(AFM)和X射线粉末衍射(XRD)。纳米晶体的特征是棒状形态,尺寸在100 nm至300 nm之间。应用于提取物纳米晶体的酸性水解作用将结晶度从72%提高到86%。获得的平均长度和直径分别为98.1±4.7和8.0±3.4nm。纤维的长径比约为12.3,低于文献中通常报道的值。动态光散射结果与显示235nm平均尺寸的纳米晶体尺寸一致。由棉制得的纤维素纳米晶须由于其含量丰富,成本低,结晶度高,强度高,重量轻和可生物降解而被纺织工业所拒绝,是加工聚合物纳米复合材料的理想选择。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号